Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Ultramid® B3WM8 BK00102 - PA6-MD40 - BASF
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center
Ultramid® 8260 HS BK-102 is generally recommended for applications such as marine hardware, brackets, fittings, bobbins, office furniture, appliance components, and power tool housings.
機械的特性 | 乾燥/調湿 | 単位 | テスト基準 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO データ | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
引張弾性率 | 6400 / 3800 | MPa | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
破壊応力 | 85 / 60 | MPa | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
破壊ひずみ | 10 / 30 | % | ISO 527 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
シャルピー衝撃強さ, +23°C | 130 / - | kJ/m² | ISO 179/1eU | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ノッチ付きシャルピー衝撃強さ, +23°C | 3 / - | kJ/m² | ISO 179/1eA |
熱的特性 | 乾燥/調湿 | 単位 | テスト基準 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO データ | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
溶融温度, 10°C/min | 220 / * | °C | ISO 11357-1/-3 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
荷重たわみ温度, 1.80 MPa | 90 / * | °C | ISO 75-1/-2 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
荷重たわみ温度, 0.45 MPa | 190 / * | °C | ISO 75-1/-2 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
厚さhでの燃焼性 | HB / * | class | IEC 60695-11-10 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
試験片の厚さ | 3.0 / * | mm | - | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
Yellow Card 可用 | はい / * | - | - |
電気的特性. | 乾燥/調湿 | 単位 | テスト基準 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO データ | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
体積抵抗率 | >1E13 / - | Ohm*m | IEC 62631-3-1 |
その他の特性. | 乾燥/調湿 | 単位 | テスト基準 |
吸水率 | 5.7 / * | % | Sim. to ISO 62 |
吸湿率 | 1.6 / * | % | Sim. to ISO 62 |
密度 | 1490 / * | kg/m³ | ISO 1183 |
injection molding, Melt temperature, range: 270 - 295 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 80 - 95 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
PREPROCESSING
Max. Water content: 0.2%
Product is supplied in sealed containers and drying prior to molding is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 80 °C (176 °F) is recommended. Drying time is dependent on moisture level.
Further information concerning safe handling procedures can be obtained from the Material Safety Data Sheet. Alternatively, please contact your BASF representative.
PROCESSING
Melt Temperature 240-280 °C (464-536 °F)
Mold Temperature 80-95 °C (176-203 °F)
Injection and Packing Pressure 35-125 bar (500-1500 psi)
A mold temperature of 80-95 °C (176-203 °F) is recommended, but temperatures of as low as 10 °C (50 °F) can be used where applicable.
Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off.
Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing.